Frits Pedersen A/S

Traceable diamonds - all diamonds has a history -

About us | Contact | Find Us | FAQ | Login
Findings Metal Gemstones and Pearls Diamonds Tools Sales Tips News Customer Center
DanskGermanPrint

Casting

ImageDescriptionAlloy
1304

925 935 585 585/Hvid 750 750/Hvid
1304

Støb

Vacumtemperatur:

935: 1050°

585: 1200°

Slyngetemperatur:

935: 1050°

585: 1050°

590*: 1250°

750: 1150°

760*: 1225°

* with 12% PD
* * * * * *
Argentium Støb

Argentium Cast

935
1307

Casting ARGENTIUM 935 tarnish resistance

Casting temp.: 970°-1040° C

Patented tarnish resistance alloy with germanium
*